| Viscosity at 25°C (cPs) |
300 ± 50 |
500 ± 50 |
| Water Content (%) |
2.20 ± 0.1 |
4.10 ± 0.1 |
| Machine Mix Reactivity |
|
|
| Component Temperature (°C) |
21 ± 1 |
21 ± 1 |
| Blended Polyol : ISO Ratio |
100 : 120 |
100 : 150 |
| Cream Time (sec) |
15 ± 2 |
15 ± 2 |
| Gel Time (sec) |
100 ± 10 |
65 ± 5 |
| Free Rise Density (kg/m³) |
27 ± 1 |
32 ± 2 |
| Physical Properties (Mold Temp. 45°C) |
|
|
| Core Density (kg/m³) |
38 ± 2 |
42 ± 2 |
| Compressive Strength (kPa) |
>100 |
>100 |
| Tensile Strength (kPa) |
>80 |
>80 |
| Dimensional Stability (-20°C, 24hr %) |
<1 |
<1 |
| Thermal Conductivity at 35°C (mW/m·K) |
0.02322 |
0.02520 |
| ODP (Ozone Depletion Potential) |
0.66 – 0.90 |
0 |
| GWP (Global Warming Potential) |
870 – 970 |
1.0 |